WE ARE EXPORTERS OF NATURAL RUBBER RSS1, 2, 3, 4, 5
1.nature rubber
2. thickening capacity
3. Excellent shear stability andthermal oxidation stability
4. free sample
5. SGS
| TSR CV | | TSR L | | TSR 5 | | TSR 10 | | TSR 20 |
|
Parameter | | Unit | | SMR CV50 | | SMR CV60 | | SMRL | | SMR 5* | | SMR GP | | SMR 10 | | SMR 10CV | | SMR 20 | | SMR 20CV |
|
Dirt (max) | | % wt | | 0.02 | | 0.02 | | 0.02 | | 0.05 | | 0.08 | | 0.08 | | 0.08 | | 0.16 | | 0.16 |
|
Ash (max) | | % wt | | 0.50 | | 0.50 | | 0.50 | | 0.60 | | 0.75 | | 0.75 | | 0.75 | | 1.00 | | 1.00 |
|
Nitrogen (max) | | % wt | | 0.60 | | 0.60 | | 0.60 | | 0.60 | | 0.60 | | 0.60 | | 0.60 | | 0.60 | | 0.60 |
|
Volatile Matter (max) | | % wt | | 0.80 | | 0.80 | | 0.50 | | 0.80 | | 0.80 | | 0.80 | | 0.80 | | 0.80 | | 0.80 |
|
Po (min) | | % wt | | NA | | NA | | 35 | | 30 | | NA | | 30 | | NA | | 30 | | NA |
|
PRI index (min) | | | | 60 | | 60 | | 60 | | 60 | | 50 | | 50 | | 50 | | 40 | | 40 |
|
Lovibond Color:individual value (max) | | | | NA | | NA | | 6.0 | | NA | | NA | | NA | | NA | | NA | | NA |
|
Lovibond Color:range (max) | | | | NA | | NA | | 6.0 | | NA | | NA | | NA | | NA | | NA | | NA |
|
Lovibond Color:range (max) | | | | NA | | NA | | NA | | NA | | NA | | NA | | NA | | NA | | NA |
|
Mooney Viscosity (ML, 1+4, 100°C) | | | | 50 +/- 5 | | 60 +/- 5 | | NA | | NA | | 65 +7/-5 | | NA | | 60 +7/-5** | | NA | | 65 +7/-5** |